1. Regarding the curling phenomenon of the coating: ① The coating is curled because there are more second-class gloss agents. ② The coating is involuted due to the excessive amount of a type of gloss agent.
2. Regarding the fragility of the coating: ① The second-category gloss agent is too high. ② Out of proportion.
3. Regarding the coating becoming black, and the edges being burnt: DK is too large.
4. Regarding the coating turning blue, and the bonding force in the recessed hole being poor: DK is too small.
"DK" means "Dry Kiln."